Exposure to chlorine based solution

More from china mfg

  • Professional aluminum Cnc Machining China
    0 commentaire , 0 comme
  • What Is 3D printing
    0 commentaire , 0 comme
  • Metal Forging
    0 commentaire , 0 comme

More in Politics

  • Norton antivirus account login
    31 commentaires, 149 860 vues
  • Liquidity Locking Made Easy
    11 commentaires, 83 791 vues
  • Ang jili178 login ay nagdudulot sa iyo ng mga laro ng slot at karanasan sa laro ng soccer
    2 commentaires, 46 843 vues

Related Blogs

  • The Advantages of Wireless CCTV Cameras for Home Security
    0 commentaire , 0 comme
  • The Benefits of Using Fog Machines in the Entertainment Industry
    0 commentaire , 0 comme
  • Top Trends in French Bulldog Clothing: What's Hot and What's Not
    0 commentaire , 0 comme

Les archives

Partage Social

Exposure to chlorine based solution

Posté par china mfg     30 mars 2022    
$211.00

Corps

Aluminum anodizing is the production of an oxide layer on the surface of aluminum parts to improve the anti-corrosion ability. we discussed this issue once. This time, we will talk about anodized aluminum coating failure. Anodizing failures of a CNC aluminum machining component generally fall into one of the following categories:

1.) Exposure to chlorine based solution

Chlorine is highly reactive and can cause corrosion on removal of the oxide layer. Be careful if the chloride ion is in a sulfuric acid electrolyte above a critical level of 80 ppm chloride. Also note that chlorine-based solvents are intended for degreasing which can also cause acid.

2.) Exposure to extremely acidic or alkaline solution

The solution lower than pH 4 or higher than pH 9 is capable of breaking up the oxide layer and making the underlying aluminum susceptible to corrosion. In general, complete rinsing of the anodized aluminum component is the most satisfactory method of eliminating this problem.

Blind holes against anodizing failure

The anodizing failure rate can be high if there are blind holes in the CNC aluminum parts. When the high acid anodizing solution is not well removed from the blind holes, the liquid will leak out and damage the surface of the CNC aluminum parts, causing them to peel and stain their anodized surface.

The photo below shows a laser cut piece of aluminum CNC engraved with acid scraps. The white, dirty, flaky oxide powder that surrounds the helical hole gradually deteriorates unless further action is taken to resolve the issue.