What Is The Definition Of Flow Marks In Lead Die Casting

More from wei long

  • You May Encounter Problems with OEM Aluminum Enclosure
    0 comments, 0 likes
  • China Zinc Die Casting Manufacturer Introduce Common Raw Materials
    0 comments, 0 likes
  • Let The Quality Of Zinc Die Casting Be Controlled
    0 comments, 0 likes

More in Politics

  • Norton antivirus account login
    31 comments, 144,863 views
  • Liquidity Locking Made Easy
    10 comments, 83,124 views
  • Ang jili178 login ay nagdudulot sa iyo ng mga laro ng slot at karanasan sa laro ng soccer
    2 comments, 46,588 views

Related Blogs

  • The Allure of Leather Lingerie: How to Embrace Your Inner Boldness
    0 comments, 0 likes
  • Decoding Thermal Imaging Colors: Understanding Their Meaning in Various Industrial Applications
    0 comments, 0 likes
  • Jaipur Shopping Tour By Rajasthan Tour Taxi Company
    0 comments, 0 likes

Archives

Social Share

What Is The Definition Of Flow Marks In Lead Die Casting

Posted By wei long     July 21, 2020    

Body

Definition of cold insulation: the surface of Lead Die Casting has obvious, irregular and sunken linear lines (penetrating and non-penetrating), with small and long shapes, some with smooth joint edges, which may develop under the action of external forces.

Causes of occurrence:

1. The two metal flows are butted with each other, but they are not completely fused and no inclusions exist between them, so the bonding force between the two metal flows is very weak.

2. The casting temperature or die casting die temperature is low.

3. Improper alloy selection and poor fluidity.

4. The casting position is wrong or the flow path is too long.

5. Low filling speed.

6. The injection ratio is low.

Definition of flow mark: There are stripes on the surface of lead die casting which are consistent with the flow direction of molten metal, and there are obvious non-directional lines which are different in color from the metal matrix, so there is no development trend.

Causes of occurrence:

1. The metal liquid entering the cavity first forms an extremely thin and incomplete metal layer, which is compensated by the later metal liquid and leaves traces.

2. The mold temperature is too low, and the mold temperature is uneven.

3. The cross-sectional area of the ingate is too small, and splashing is caused by improper position.

4. Insufficient pressure acting on molten metal.

5. Too much pattern and coating.

We are also a professional China Die Casting Factory, if necessary, please contact us.