Production Problems and Solutions of Zinc Die Castings

More from wei long

  • You May Encounter Problems with OEM Aluminum Enclosure
    0 comentarios, 0 likes
  • China Zinc Die Casting Manufacturer Introduce Common Raw Materials
    0 comentarios, 0 likes
  • Let The Quality Of Zinc Die Casting Be Controlled
    0 comentarios, 0 likes

More in Politics

  • Norton antivirus account login
    31 comentarios, 148.059 vistas
  • Liquidity Locking Made Easy
    11 comentarios, 83.630 vistas
  • Ang jili178 login ay nagdudulot sa iyo ng mga laro ng slot at karanasan sa laro ng soccer
    2 comentarios, 46.775 vistas

Related Blogs

  • La nueva equipaci\u00f3n del FC Barcelona 2024: Una mirada a la evoluci\u00f3n del dise\u00f1o
    0 comentarios, 0 likes
  • Tips When Getting Natural Leather Sofas
    0 comentarios, 0 likes
  • Transform Your Workspace with ARIRA BuildTech Private Limited - The Premier Office Renovation Company
    0 comentarios, 0 likes

Archivo

compartir social

Production Problems and Solutions of Zinc Die Castings

Publicado por wei long     29 de diciembre de 2020    

Cuerpo

Die casting is a kind of pressure casting part. It uses a pressure casting machine die casting machine equipped with a casting mold to pour liquid copper, zinc, aluminum, or aluminum alloy into the inlet of the die casting machine and pass it through the die casting machine. Die casting is to cast copper, zinc, aluminum parts, or aluminum alloy parts of the shape and size restricted by the mold. Such parts are usually called die castings. However, in the process of producing zinc die casting , there will be many problems. Now let's take a look at the problems and solutions in the production of die-casting parts.

During production, if the surface of the casting swells with micro-cracks, it is a phenomenon that the alloy composition meets the requirements but a large number of pores appear, then the cause of the defect may be the premature opening of the mold or the mold temperature may be too high. There are likely a lot of bubbles inside the casting. When the metal solidification time is not enough, the strength is not established, and the mold is opened prematurely to eject the casting. The pressure bubbles expand and the surface of the casting is raised and hot cracks are generated. The solution is not without, we adjust the process parameters in the die-casting process to keep the mold longer and reduce the mold temperature in the defect area.

The above is the solution to the phenomenon that the surface of the casting swells and has micro-cracks, but we will have other problems when we produce lead die casting or other die castings, so we still need the accumulation of experience and the precipitation of time, so Don't be too hasty, slowly accumulate little by little.